Physical Property Data Comparing Various Hi-Strength
Epoxies to System 2000 Epoxy Resin

Brand Name |
System 2000 |
Saf-T-Poxy |
Epolite |
EZ Poxy |
RAE |
West
Systems
ProSet |
Test Method |
PRODUCT |
2000
w/2020 |
2000
w/2060 |
2000
w/2120 |
2410
w/2183 |
2410
w/2184 |
2427
|
EZ10
w/EZ83 |
2426
w/2177 |
125R
w/229H |
|
Mix Ratio
By weight
By volume |
100:23
4.3:1
|
100:27
3:1
|
100:27
3:1
|
100:44
2.13:1
|
100:44
2.13:1
|
100:44
2.13:1
|
100:44
2.13:1
|
100:21
4:1
|
100:30
2.86:1
|
Literature |
Mixed Viscosity, centipoise |
950-975 |
900 |
925 |
1300 |
800 |
700 |
750 |
680 |
325 |
ASTM D2293 |
Pot-Life @ 77°F,
4 fl. Oz. |
20 min |
1 hr. |
2 hr. |
2 hr. |
2 hr. |
2 hr. |
2 hr. |
1 hr. |
1.5 hr. |
ASTM D2471 |
Cured Hardness,
Shore D |
88 D |
88 D |
87 D |
88 D |
85 D |
86 D |
88 D |
89 D |
89 D |
ASTM D2240 |
Specific Gravity |
1.12-1.13 |
1.11 |
1.12 |
1.14 |
1.13 |
1.15 |
1.18 |
1.15 |
1.15 |
ASTM D1475 |
Density
lb./cu. in.
lb./gallon |
.0410
9.47
|
.0401
9.26
|
.0410
9.34
|
.0412
9.51
|
.0409
9.43
|
.0415
9.60
|
.0428
9.85
|
.0415
9.60
|
.0415
9.60
|
ASTM D792 |
Tensile Strength, psi |
45,326 |
45,170 |
45,870 |
39,280 |
38,940 |
32,080 |
40,870 |
39,880 |
42,810 |
ASTM D638 |
Elongation @ Break, % |
1.93% |
1.96% |
1.98% |
1.83% |
2.04% |
1.62% |
1.97% |
1.87% |
2.04% |
ASTM D638 |
Tensile Modulus, psi |
2,530,000 |
2,620,000 |
2,520,000 |
2,160,000 |
2,140,000 |
2,000,000 |
2,130,000 |
2,440,000 |
2,430,000 |
ASTM D638 |
Flexural Strength, psi |
65,308 |
62,285 |
66,667 |
46,856 |
42,028 |
30,401 |
44,814 |
54,344 |
55,561 |
ASTM D790 |
Flexural Modulus, pzi |
2,830,000 |
2,560,000 |
3,050,000 |
2,410,000 |
2,240,000 |
2,130,000 |
2,830,000 |
2,780,000 |
2,840,000 |
ASTM D790 |
Glass Transition Temp. (Tg) |
180°F |
196°F |
194°F |
184°F |
182°F |
140°F |
148°F |
145°F |
146°F |
TMA |

|